Polymer Property : Tensile Modulus = 11.724 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 11.724 GPa
1700.4 ksi
ASTM D-638
PlastiComp Complet® LGF50-PA12 Nylon 12, 50% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 12 with 50% long glass fiber reinforcementInformation provided by PlastiComp, In..