Mechanical Properties Metric English Comments
Tensile Modulus 6.00 - 8.00 GPa
870 - 1160 ksi
DIN 53457
Schwartz Technical Plastics LAMINEX® 2140 Cotton Fabric, Phenolic Resin Impregnated, MoS2 Filled
Application: bearing shells and bearing collarsInformation provided by Schwartz Technical Plastics GmbH
Tensile Modulus 6.00 - 8.00 GPa
870 - 1160 ksi
DIN 53457
Schwartz Technical Plastics LAMINEX® 2100 Cotton Fabric, Phenolic Resin Impregnated
Application: bearing shells and bearing collarsInformation provided by Schwartz Technical Plastics GmbH