Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 125 GPa | 18100 ksi | |
Hexcel® HexPly® EH04 Epoxy Resin System, AS4C Fiber AS4C 150 24" EH04 35%; Normalized to 55% fiber volume; 75°F, dryInformation provided by HexCel |
|||
Tensile Modulus | 125 GPa | 18100 ksi | Young's; DINV ENV 843-2 / ASTM-F417 |
CeramTec 447 Cordierite, 2MgO•Al2O3•5SiO2 Cordierites have low coefficients of thermal expansion and excellent resistance to thermal shock. They offer a range of thermal expansion, mechanical strength, and porosity criteria. They excel as c.. |