Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 13.21 GPa | 1916 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP VERTON RV008ES PA 66 LNP* VERTON* RV008ES is a compound based on Nylon 66 resin containing 40% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural. |
|||
Tensile Modulus | 13.21 GPa | 1916 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP VERTON RV008ES PA 66 (Asia Pacific) LNP* Verton* RV008ES is a compound based on Nylon 66 resin containing Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized. |