Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 1916 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 13.21 GPa
1916 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP VERTON RV008ES PA 66
LNP* VERTON* RV008ES is a compound based on Nylon 66 resin containing 40% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural.
Tensile Modulus 13.21 GPa
1916 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP VERTON RV008ES PA 66 (Asia Pacific)
LNP* Verton* RV008ES is a compound based on Nylon 66 resin containing Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized.
Copyright © lookpolymers.com All Rights Reserved