Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.940 GPa | 136 ksi | At 1 mm/min; ISO 527-2 |
Borealis Daplen™ KSR4525 Polypropylene Reactor Elastomer Modified Daplen KSR4525 is a reactor elastomer modified polypropylene intended for injection molding. Daplean KSR4525 is a material with excellent impact/stiffness ratio. The grade is available in natural .. |
|||
Tensile Modulus | 0.940 GPa | 136 ksi | TD; ASTM D882-A |
Borealis FL5580 High Density Polyethylene FL5580 is a high density polyethylene with an excellent combination of extrusion properties and moisture barrier properties. Applications: FL5580 has been developed especially for applications like.. |
|||
Tensile Modulus | 0.940 GPa | 136 ksi | ISO 527-1/-2 |
Unitika A1030BRL PA6, Conditioned Information provided by Unitika Ltd. |
|||
Tensile Modulus | 0.938 GPa | 136 ksi | ASTM D638 |
Westlake Plastics Ultra Ethylux® HDPE Ultra Ethylux is made from high density polyethylene resin. This material is a cost effective alternative for a variety of end uses including mild chemical and wear applications. Information provid.. |
|||
Tensile Modulus | 0.940 GPa | 136 ksi | ISO 527-1/-2 |
Unitika A1030SR PA6, Conditioned Information provided by Unitika Ltd. |
|||
Tensile Modulus | 0.940 GPa | 136 ksi | cond; ISO 527-1/-2 |
DSM EcoPaXX® Q-X07207 PA410-I Impact Modified |
|||
Tensile Modulus | 0.940 GPa | 136 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® R 47 HW 10 PA6 Grilon R 47 HW 10 is a flexible, cold impact resistant and heat stabilized polyamide 6 for applications in the extrusion. The material can be processed on all for polyamides suitable tube-extrusion .. |
|||
Tensile Modulus | 0.936 GPa @Temperature 120 °C |
136 ksi @Temperature 248 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 73M40 NC010 Nylon 6
(Unverified Data**) 40% Mineral Reinforced Polyamide 6 Minlon 73M40 NC010 is a 40% mineral reinforced heat stabilized polyamide 6 resin for injection molding. It has isotropic properties and low warpage.Information pro.. |