Polymer Property : Tensile Modulus = 14.0 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.0965 GPa
14.0 ksi
ASTM D638
3M Dyneon™ CCX6380 PTFE, 10% Polyimide Filler  (discontinued **)
Type II, free flowing.Typical Applications: Finished or semi-finished parts: sheets, rods, tubes, billets for skiving of films or machining into complex shapes.Information provided by the Dyneon div..
Tensile Modulus 0.0965 GPa
14.0 ksi
ASTM D638
3M Dyneon™ TF 4103 PTFE 15% Glass Fiber Filled  (discontinued **)
Type II PTFE. Applications include valve seats, bearings, seals/gaskets, moldings, piston rings.Data provided by Dyneon.