Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 14.78 GPa | 2144 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP VERTON RV0079 PA 66 LNP VERTON* RV0079 is a compound based on Nylon 66 resin containing 35% Long Glasss Fiber. Added features of this material include: Flame Retardant, Structural. |