Mechanical Properties Metric English Comments
Tensile Modulus 14.78 GPa
2144 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP VERTON RV0079 PA 66
LNP VERTON* RV0079 is a compound based on Nylon 66 resin containing 35% Long Glasss Fiber. Added features of this material include: Flame Retardant, Structural.