Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 15.87 GPa | 2302 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP DC006 PC (Asia Pacific) LNP THERMOCOMP* DC006 is a compound based on Polycarbonate resin containing Carbon Fiber.This product is also known as Thermocomp* DC-1006. |