Polymer Property : Tensile Modulus = 2302 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 15.87 GPa
2302 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP DC006 PC (Asia Pacific)
LNP THERMOCOMP* DC006 is a compound based on Polycarbonate resin containing Carbon Fiber.This product is also known as Thermocomp* DC-1006.