Mechanical Properties Metric English Comments
Tensile Modulus 10.92 GPa
1584 ksi
ASTM D638
Plenco 50130 PET, Pellet, Injection Molded, Natural Color  (discontinued **)
PLENCO 50130 is an engineering grade glass reinforced UL flame rated polyethylene terephthalate resin designed for good physical strength. It is UL listed and available in natural and black.Informat..