Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 11.48 GPa
1665 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP UX95672 PPA
LNP LUBRICOMP* UX95672 is a compound based on Polyphthalamide resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant.
Tensile Modulus 11.48 GPa
1665 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP PFW64 PA 6
LNP* THERMOCOMP* PFW64 is a compound based on Nylon 6 resin containing 20% Glass Fiber, 30% Wollastonite.