Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 17.07 GPa | 2476 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP 5CL24 PVDF LNP* Lubricomp* 5CL24 is a compound based on Polyvinylidene Fluoride resin containing 10% PTFE and 20% Carbon Fiber. Added features of this material include: Internally Lubricated. |