Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 17.4 GPa | 2530 ksi | Property derived with 10 Ply Laminate, hand Lay-up, Style 181 Glass Fabric, 55% Glass Content. |
Fibre Glast 2000 / 2020 System 2000 Epoxy System 2000 Epoxy Resin is a low viscosity, light amber laminating resin that is designed for fabricating parts and other demanding structural applications. Use this system to maximize the physical .. |
|||
Tensile Modulus | 17.4 GPa | 2520 ksi | Property derived with 10 Ply Laminate, hand Lay-up, Style 181 Glass Fabric, 55% Glass Content. |
Fibre Glast 2000 / 2120 System 2000 Epoxy System 2000 Epoxy Resin is a low viscosity, light amber laminating resin that is designed for fabricating parts and other demanding structural applications. Use this system to maximize the physical .. |
|||
Tensile Modulus | 17.4 GPa | 2520 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RFN1ASXS PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RFN1ASXS is a compound based on Nylon 66 resin containing Glass Fiber, MOS2. Added features of this material include: Heat Stabilized. |
|||
Tensile Modulus | 17.4 GPa | 2520 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP DF00A1P PC (Asia Pacific) LNP* Thermocomp* DF00AIP is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High Modulus, low warpage, Non-Brominated & Non.. |
|||
Tensile Modulus | 17.4 GPa | 2520 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TSGL-50-4 nat PA666-GF50 Product description: Grilon TSGL-50/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 50% long glass fibers. Grilon TSGL-50/4 natural is characterized by the following .. |