Polymer Property : Tensile Modulus = 1735 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 11.96 GPa
1735 ksi
ASTM D638
Plenco 50240 PET, Pellet, Injection Molded, Natural Color  (discontinued **)
PLENCO 50240 is an engineering grade glass reinforced UL flame rated polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in natural and black..
Tensile Modulus 11.96 GPa
1735 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP OF006 PPS - Linear
LNP* THERMOCOMP* OF006 is a compound based on Linear PPS containing 30% Glass Fiber.
Tensile Modulus 11.96 GPa
1735 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP PF007 PA 6
LNP* THERMOCOMP* PF007 is a compound based on Nylon 6 resin containing 35% Glass Fiber.
Tensile Modulus 11.96 GPa
1735 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP D452 PC COPOLYMER (Asia Pacific)
LNP* Thermocomp* D452 (or EXTC8202) is a compound based on SABIC unique Polycarbonate copolymer resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, ..
Tensile Modulus 11.96 GPa
1735 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Thermocomp PF007 PA 6 (Asia Pacific)
LNP* Thermocomp* PF007 is a compound based on Nylon 6 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
Tensile Modulus 11.96 GPa
1735 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP VERTON PX06418 PA 6
LNP* VERTON* PX06418 is a compound based on Nylon 6 containing proprietary fillers. Added features of this grade are: Heat Stabilized, Structural.