LNP* THERMOCOMP* PF007 is a compound based on Nylon 6 resin containing 35% Glass Fiber.
Physical Properties Metric English Comments
Density 1.43 g/cc
0.0517 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0080 cm/cm

@Time 86400 sec
0.0080 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 173 MPa
25100 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Tensile Modulus 11.96 GPa
1735 ksi
50 mm/min; ASTM D638
Flexural Strength 255 MPa
37000 psi
ASTM D790
Flexural Modulus 9.14 GPa
1330 ksi
ASTM D790
Izod Impact, Notched 1.44 J/cm
2.70 ft-lb/in
ASTM D256
Izod Impact, Unnotched 12.22 J/cm
22.89 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 205 °C

@Thickness 3.20 mm
401 °F

@Thickness 0.126 in
unannealed; ASTM D648