Polymer Property : Tensile Modulus = 19.42 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 19.42 GPa
2817 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP SCL36 PA12
LNP* LUBRICOMP* SCL36 is a compound based on Nylon 12 resin containing 15% PTFE, 30% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive.
Tensile Modulus 19.42 GPa
2817 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP QC006I PA 6/10
LNP THERMOCOMPâ„¢ QC006I is a compound based on Nylon 6/10 containing 30% Carbon Fiber. Added features of this grade include: High Impact.