Mechanical Properties Metric English Comments
Tensile Modulus 2.66 GPa
386 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Packaging PK9 WHITE 1082 Polyvinyl Chloride, Rigid (PVC, Rigid)
The HDT value refers to samples conditioned @ 50 deg.C. for 24 hrs.The bulk density test was performed under ASTM D-1895B.Information provided by PolyOne
Tensile Modulus 2.66 GPa
386 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® SLX1432D PC Copolymer
Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Americas region.
Tensile Modulus 2.66 GPa
386 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® SLX1432D PC Copolymer (Asia Pacific)
Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region.
Tensile Modulus 2.66 GPa
386 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® SLX1432D PC Copolymer (Europe-Africa-Middle East)
Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Tensile Modulus 2.66 GPa
386 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® SLX2432D PC Copolymer
Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Americas region.
Tensile Modulus 2.66 GPa
386 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® SLX2432D PC Copolymer (Asia Pacific)
Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region.
Tensile Modulus 2.66 GPa
386 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Lexan® SLX2432D PC Copolymer (Europe-Africa-Middle East)
Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East reg..
Tensile Modulus 2.66 GPa
386 ksi
same value from ASTM and ISO test.
BASF Capron® GR15 HS 15% Glass-Filled Nylon 6 (Conditioned)  (discontinued **)
Capron GR15 HS is a heat stabilized 15% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aest..
Tensile Modulus 2.66 GPa
386 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Lexan® SLDM310 PC (Asia Pacific)
Mineral filled Antistatic Polycarbonate, HDT110degC type
Tensile Modulus 2.66 GPa
386 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics XYLEX X7507 PC+POLYESTER
F-1 weathering certified in natural color, specially designed for Pool & Spa applications.
Tensile Modulus 2.66 GPa
386 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics XYLEX X7507 PC+POLYESTER (Asia Pacific)
F-1 weathering certified in natural color, specially designed for Pool & Spa applications. Currently available in natural color only.
Tensile Modulus 2.66 GPa
386 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics XYLEX X7507 PC+POLYESTER (Europe-Africa-Middle East)
F-1 weathering certified in natural color, specially designed for Pool & Spa applications. Currently available in natural color only.
Tensile Modulus 2.66 GPa
386 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP 9X10401H ABS
LNP* THERMOCOMP* 9X10401H is a compound based on Polyphenylsulfone containing proprietary filler(s). Added feature of this grade is: X-Ray Opaque.
Tensile Modulus 2.66 GPa

@Temperature 120 °C
386 ksi

@Temperature 248 °F
ISO Data
BASF Ultramid® 8333G HI 33% Glass Filled PA6 (Dry)
Ultramid 8333G HI is a 14% glass reinforced, impact modified PA6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a balance of st..
Tensile Modulus 2.66 GPa
386 ksi
same value from ASTM and ISO test.
BASF Capron® GR15 15% Glass-Filled Nylon 6 (Conditioned)  (discontinued **)
Capron GR15 is a 15% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aesthetics. It is also..