Mechanical Properties Metric English Comments
Tensile Modulus 14.50 GPa
2103 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Therma-Tech™ NJC-7500 Nylon 12  (discontinued **)
PolyOne First ChoiceInformation provided by PolyOne Corporation.