Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Therma-Tech™ NJC-7500 Nylon 12  (discontinued **)

Category Polymer , Thermoplastic , Nylon , Nylon 12
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Therma-Tech™ NJC-7500 Nylon 12  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.677 g/cc
1.677 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 39.61 MPa
5745 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Elongation at Break 0.4272 %
0.4272 %
Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 14.50 GPa
2103 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Strength 68.83 MPa
9983 psi
ASTM D790
Flexural Modulus 11.42 GPa
1656 ksi
ASTM D790
Izod Impact, Notched 0.184 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
0.345 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
Thermal Properties Metric English Comments
Thermal Conductivity >= 25.00 W/m-K
>= 173.5 BTU-in/hr-ft²-°F
ASTM C177
Electrical Properties Metric English Comments
Surface Resistivity per Square 49000 ohm
49000 ohm
ASTM D257
Descriptive Properties Value Comments
Product Form Pellets
Users viewing this material also viewed the following: