Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.527 GPa @Temperature 150 °C |
221.5 ksi @Temperature 302 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9330 NC010 PBT+SAN
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9330 NC010 is a 30% glass fiber reinforced polybutylene terephthalate blend for injection molding. I.. |