Polymer Property : Tensile Modulus = 231 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 1.59 GPa
231 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne LubriOne™ PC-000/10T Polycarbonate (PC)
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
Tensile Modulus 1.59 - 1.66 GPa
231 - 241 ksi
ASTM D638
Proto3000 Accura® 25 Plastic Stereolithography (SLA) Prototyping Polymer
Description: A high stiffness engineered nanocomposite that opens new applications for stereolithography users. Features: Look and feel of molded polypropyleneOutstanding feature resolution and accu..
Tensile Modulus 1.59 GPa
231 ksi
ASTM Data
Dow Isoplast® 151 Polyurethane (PUR-RT), Impact Modified  (discontinued **)
ISOPLAST® 151 resin is an impact modified amorphous polymer with the chemical resistance of crystalline resins. Its outstanding properties include excellent chemical resistance, high heat, low mois..
Tensile Modulus 1.59 GPa
231 ksi
1mm/min
Eastman Tenite 371A-12 CAP Cellulose Acetate Propionate  (discontinued **)
12% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical.
Tensile Modulus 1.59 GPa
231 ksi
1mm/min
Eastman Tenite 264-10 CAB Cellulose Acetate Butyrate  (discontinued **)
10% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical.
Tensile Modulus 1.59 GPa
231 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-LOY K3000SZ Acetal Copoly
LNP* STAT-LOY* K3000SZ is a compound based on Acetal Copolymer resin. Added feature of this material is: AntiSstatic.
Tensile Modulus 1.59 GPa
231 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-LOY K3000SZ Acetal Copoly (Asia Pacific)
LNP* Stat-loy* K3000SZ is a compound based on Acetal Copolymer resin containing Anti-Static. Added features of this material include: Antistat.
Tensile Modulus 1.59 GPa
231 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-LOY K3000Z Acetal
LNP* STAT-LOY* K3000Z is a compound based on unfilled Acetal resin. Added feature of this material is: Antistat.
Tensile Modulus 1.59 - 1.66 GPa
231 - 241 ksi
ASTM D638
3D Systems Accura® 25 Plastic for SLA® Systems
For use with solid-state stereolithography (SLA®) systems.ApplicationsFunctional components for assemblies and mock-ups for:Automotive styling parts — trim, fascia, and other componentsConsumer el..