Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 2580 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 17.8 GPa
2580 ksi
ISO 527-2
Solvay Specialty Polymers Kalix® 2955 Polyamide, High Performance (HPPA), Glass Fiber
Kalix® 2955 is a 27% bio-sourced, PA 6,10-based compound with 55% by weight glass fiber reinforcement. This material is specifically formulated for high strength and stiffness applications where ..
Tensile Modulus 17.8 GPa
2580 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP VERTON RV00AES PA 66 (Europe-Africa-Middle East)
LNP VERTON* RV00AES is a compound based on PA 66 resin containing Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized.
Tensile Modulus 17.8 GPa
2580 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Verton RV00AESM PA 66 (Europe-Africa-Middle East)
LNP* VERTON* RV00AESM is a compound based on PA66 resin containing Long Glass Fiber. Added features include: Easy Moldin, Heat Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-Mid..
Tensile Modulus 17.8 GPa
2580 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP VERTON RV00AESP PA 66 (Europe-Africa-Middle East)
LNP* VERTON* RV00AESP is a compound based on PA66 resin containing Long Glass Fiber. Added features include : Easy Molding, Heat Stabilized.
Tensile Modulus 17.8 GPa
2580 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP VERTON RV00AESS PA 66 (Europe-Africa-Middle East)
LNP* VERTON* RV00AESS is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Easy Molding, Heat Stabilized.
Tensile Modulus 17.8 GPa
2580 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP VERTON RV00AEU PA 66 (Europe-Africa-Middle East)
LNP* VERTON* RV00AEU is a compound based on PA 66 resin containing Long Glass Fiber. Added features include : Easy Molding, UV Stabilized.
Tensile Modulus 17.8 GPa
2580 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP VERTON RV00AEX5 PA6.6 (Europe-Africa-Middle East)
LNP* VERTON* Is a compound based on PA66 resin containing Long Glass Fiber. Added features include: Easy Molding, Heat Stabilized.
Tensile Modulus 17.8 GPa
2580 ksi
dry; ISO 527-1/-2
EMS-Grivory Grivory® TSGL-50/4 black 9833 PA666-GF50
Product description: Grilon TSGL-50/4 black is based on a heat stabilized semicrystalline Polyamide PA66+PA6 and 50% long glass fibers. Grilon TSGL-50/4 black is characterized by the following key-p..