Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 27.6 GPa | 4000 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ SF2-30CF/15T Natural Polyphenylene Sulfide (PPS) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Modulus | 27.6 GPa | 4000 ksi | RT, Dry, 90° Direction |
Renegade Materials Corporation MVK-14 Polyimide FreeForm™ Astroquartz 4581 Fabric MVK-14 Polyimide Astroquartz and S2 glass prepregs are an affordable, easy-to-process material for high-temperature radome and antenna applications. MVK-14 is a non-MDA alternative to BMI, cyanate e.. |
|||
Tensile Modulus | 27.6 GPa | 4000 ksi | RT, Dry, 90° Direction |
Renegade Materials Corporation MVK-14 Polyimide FreeForm™ S2-Glass Fabric MVK-14 Polyimide Astroquartz and S2 glass prepregs are an affordable, easy-to-process material for high-temperature radome and antenna applications. MVK-14 is a non-MDA alternative to BMI, cyanate e.. |
|||
Tensile Modulus | 27.6 GPa | 4000 ksi | ASTM D638 |
PolyOne Edgetek® LCP-30CF/000 Liquid Crystal Polymer - 30% Carbon Fiber
(discontinued **) Data provided by PolyOne. |
|||
Tensile Modulus | 27.6 GPa | 4000 ksi | ASTM D3039 |
Greene Tweed Orthetek® RP Polyketone, Random Carbon Fiber Greene Tweed offers precision-molded thermoplastic components made form out high-performance Orthtek® composite materials for a variety of demanding medical device applications. Orthtek RP is id.. |