Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Greene Tweed Orthetek® RP Polyketone, Random Carbon Fiber

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Carbon Fiber Filled
Manufacturer Greene Tweed
Trade Name Orthetek®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Greene Tweed Orthetek® RP Polyketone, Random Carbon Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Greene Tweed offers precision-molded thermoplastic components made form out high-performance Orthtek® composite materials for a variety of demanding medical device applications. Orthtek RP is ideally suited to replace metal due to strength, dimensional stability, low weight and corrosion resistance. Orthtek RP is recommended for noncomplex parts such as nail guides where radiolucentcy and autoclaving are required.Applications:Medical Trauma – Targeting instruments such as tibial or humeral nail guidesMedical Orthopedic – Surgical instruments and retractorsInformation provided by Greene Tweed.
Physical Properties Metric English Comments
Specific Gravity 1.54 g/cc
1.54 g/cc
ASTM D792
Water Absorption 0.050 %
0.050 %
at 212°F (100°C); ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1240 MPa
180000 psi
ASTM D3039
Elongation at Break 0.50 %
0.50 %
ASTM D3039
Tensile Modulus 27.6 GPa
4000 ksi
ASTM D3039
Flexural Strength 324 MPa
47000 psi
ASTM D790
Flexural Modulus 25.5 GPa
3700 ksi
ASTM D790
Compressive Strength 255 MPa
37000 psi
ASTM D695
Compressive Modulus 22.8 GPa
3300 ksi
ASTM D695
Descriptive Properties Value Comments
Color Black
Fiber Orientation Random
Fiber Volume, % 50