Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.915 GPa | 277.7 ksi | ASTM D638 |
Proto3000 ABSi Fused Deposition Modeling Polymer Description: Stratasys ABSi is an ideal material for conceptual modeling, functional prototyping and direct digital manufacturing. Its strength is superior to standard Stratasys ABS, and the translu.. |
|||
Tensile Modulus | 1.915 GPa | 277.7 ksi | ASTM D638 |
Stratasys® ABSi Stratasys is the only company that gives engineers the ability to manufacture real ABSi industrial thermoplastic parts direct from digital files. ABSi parts can be used from conceptual prototyping t.. |