Mechanical Properties Metric English Comments
Tensile Modulus 19.1 GPa
2770 ksi
Type I, 5.0 mm/min; ISO 527
PolyOne LubriOne™ NN-30CF/15T-02S black Polyamide 66 (Nylon 66)
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
Tensile Modulus 19.1 GPa
2770 ksi
ISO 527-2
Solvay Specialty Polymers Amodel® FC-1150 Polyphthalamide (PPA), 50% Glass Fiber
Amodel® FC-1150 is an FDA-approved, 50% glass fiber reinforced resin designed for high strength and stiffness. This combines with its excellent thermal properties, low water absorption and good h..