Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 192 GPa | 27900 ksi | |
Carpenter AerMet® 340 |
|||
Tensile Modulus | 192 GPa | 27900 ksi | |
Carpenter AerMet® 100 Aged at 875°F An alloy providing high hardness and strength combined with exceptional ductility and toughness. This alloy should be considered for aircraft and aerospace structural components requiring high stren.. |
|||
Tensile Modulus | 192 GPa | 27900 ksi | |
Carpenter AerMet® 310 AerMet 310 alloy possesses higher hardness and strength than AerMet 100 alloy while maintaining exceptional ductility and toughness. At a 310 ksi (2137 MPa) ultimate tensile strength, AerMet 310 all.. |