Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 28.3 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.195 GPa
28.3 ksi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® XE 3982 PA12
Product description: Grilamid XE 3982 is a highly flexible extrusion grade, based on Polyamide 12 with following main attributes: High flexibilityLow plasticizer migration (low blooming)Very good ch..
Tensile Modulus 0.195 GPa
28.3 ksi
dry; ISO 527-1/-2
EMS-Grivory Grivory® XE 3982 PA12
Product description: Grilamid XE 3982 is a highly flexible extrusion grade, based on Polyamide 12 with following main attributes: High flexibilityLow plasticizer migration (low blooming)Very good ch..
Tensile Modulus 0.195 GPa
28.3 ksi
1 mm/min
Arkema Group Rilsan® BMV 400 TL Nylon 11 (Dry)
Designation ISO 1874-PA11,M,18-002,ZFlexible grade for injection molding. Available color: natural. Light and heat stabilized. Plasticizing agent free.Outstanding impact strength and tear spreading ..
Copyright © lookpolymers.com All Rights Reserved