Material Notes:
Product description: Grilamid XE 3982 is a highly flexible extrusion grade, based on Polyamide 12 with following main attributes: High flexibilityLow plasticizer migration (low blooming)Very good chemical resistanceGood light and heat stabilityGood dimensional stability Application examples: Flexible hoses and profiles, pneumatic tubes.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 0.990 g/cc
0.0358 lb/in³
ISO 1183
Water Absorption 1.2 %
1.2 %
ISO 62
Moisture Absorption 0.500 %
0.500 %
ISO 62
Linear Mold Shrinkage, Flow 0.0060 cm/cm
0.0060 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.014 cm/cm
0.014 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Hardness, Shore D 53
53
conditioned, 15s; ISO 868
Ball Indentation Hardness 20.0 MPa
2900 psi
conditioned; ISO 2039-1
Tensile Strength at Break 40.0 MPa
5800 psi
conditioned; ISO 527-1/-2
45.0 MPa
6530 psi
dry; ISO 527-1/-2
Tensile Stress 18.0 MPa

@Strain 50.0 %
2610 psi

@Strain 50.0 %
conditioned; ISO 527-1/-2
18.0 MPa

@Strain 50.0 %
2610 psi

@Strain 50.0 %
dry; ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
dry; ISO 527-1/-2
>= 50 %
>= 50 %
conditioned; ISO 527-1/-2
Tensile Modulus 0.195 GPa
28.3 ksi
conditioned; ISO 527-1/-2
0.195 GPa
28.3 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched NB
NB
dry; ISO 179/1eU
NB
NB
conditioned; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
dry; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched NB
NB
dry; ISO 179/1eA
NB
NB
conditioned; ISO 179/1eA
0.900 J/cm²

@Temperature 30.0 °C
4.28 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
1.00 J/cm²

@Temperature 30.0 °C
4.76 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 160 µm/m-°C
88.9 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 160 µm/m-°C
88.9 µin/in-°F
ISO 11359-1/-2
Melting Point 170 °C
338 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 80.0 - 110 °C
176 - 230 °F
long term; EMS
150 °C
302 °F
short term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C
176 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
conditioned; IEC 60093
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
IEC 60093
Dielectric Strength 39.0 kV/mm
991 kV/in
conditioned; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Additives Plasticizer
Electricals & Electronics Cables & Tubes
Form Granules
Industry & Consumer goods Hydraulics & Pneumatics
Processing Other Extrusion
Product Attributes Flexible
Special Characteristics High impact or impact modified
Improved UV resistance (outdoor use)