Mechanical Properties Metric English Comments
Tensile Modulus 20.36 GPa
2953 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP RF00C PA 66
LNP THERMOCOMP* RF00C is a compound based on Nylon 66 resin containing 60% Glass Fiber.
Tensile Modulus 20.36 GPa
2953 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Verton UV00A PPA
LNP VERTON* UV00A is a compound based on Polyphthalamide resin containing Long Glass.This data was supplied by SABIC-IP for the Americas region.
Tensile Modulus 20.36 GPa
2953 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Verton UV00A PPA (Asia Pacific)
LNP VERTON* UV00A is a compound based on Polyphthalamide resin containing Long Glass.This data was supplied by SABIC-IP for the Asia Pacific region.