Mechanical Properties Metric English Comments
Tensile Modulus 20.68 GPa
2999 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON Noryl_NC2525 PPE+HIPS (Europe-Africa-Middle East)
LNP* Stat-kon* Noryl_NC2525 compound is a 25% CFR PPE+PS. Highly conductive. High heat. May be added to similar material/regrind to add some conductivity to the blend.
Tensile Modulus 20.68 GPa
2999 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON Noryl_NC2525 PPE+PS
LNP* Stat-kon* Noryl_NC2525 compound is a 25% CFR PPE+PS. Highly conductive. High heat. May be added to similar material/regrind to add some conductivity to the blend.
Tensile Modulus 20.68 GPa
2999 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Lubricomp KCL36 Acetal Copoly
LNP* Lubricomp* KCL36 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data ..
Tensile Modulus 20.68 GPa
2999 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP KCL36 Acetal Copoly (Asia Pacific)
LNP* Lubricomp* KCL36 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.
Tensile Modulus 20.68 GPa
2999 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON EX99550C PEI
LNP* STAT-KON* EX99550C is a compound based on Polyetherimide resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive.