Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.20 - 3.38 GPa | 464 - 490 ksi | ASTM D638 |
Proto3000 Accura® 55 Plastic Stereolithography (SLA) Prototyping Polymer Simulate the look and feel of molded ABS with this tough and versatile plastic.Features:Durable and rigid materialLook and feel of molded ABSHigh accuracy with less distortionHigh production speedLo.. |
|||
Tensile Modulus | 3.20 - 3.38 GPa | 464 - 490 ksi | ASTM D638 |
3D Systems Accura® 55 Plastic for SLA® Systems Simulate the properties and appearance of molded ABS. For use with solid-state stereolithography (SLA®) systems.ApplicationsAutomotive interior componentsShort-run production partsElectronic compon.. |