Mechanical Properties Metric English Comments
Tensile Modulus 3.55 GPa
515 ksi
1 mm/min
Polimeri Europa KOSTIL B266 Styrene Acrylonitrile
Symbol according to ISO 1043-1: SAN Grade designation according to ISO 4894-SAN 2,M,105-15 Standard injection moulding grade with good chemical resistance Application fields: household and small ..
Tensile Modulus 3.55 - 3.65 GPa
515 - 529 ksi
ASTM D638
Prodways PLASTCure ABS 3650 3D Printing Polymer
Good chemical resistance. High transparency.Ideal for segments such like medical, electronic, aerospace and automotive markets that demand accurate RTV patterns, durable concept models, highly accur..
Tensile Modulus 3.55 GPa
515 ksi
ISO 527-1/-2
Quadrant EPP Ertalon® 66 SA PA 66, extruded (ISO Data)
Material with a higher mechanical strength, stiffness, heat and wear resistance than Ertalon 6 SA. It also has a better creep resistance but its impact strength and mechanical damping ability is red..
Tensile Modulus 3.55 GPa
515 ksi
ISO 527-1/2
Radici Radilon® AHS (dry) Nylon 66
General purposeInformation provided by Radici group.
Tensile Modulus 3.55 GPa
515 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Valox® K4530 PBT (Europe-Africa-Middle East)
15% glass reinforced PBT, Hydrolytically stable, High flow, Automotive connectors.
Tensile Modulus 3.55 GPa
515 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Thermocomp KB002 Acetal Copoly
LNP* Thermocomp* KB002 is a compound based on Acetal Copolymer resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region.
Tensile Modulus 3.55 GPa
515 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Thermocomp KB002 Acetal Copoly (Asia Pacific)
LNP* Thermocomp* KB002 is a compound based on Acetal Copolymer resin containing Glass Bead.This data was supplied by SABIC-IP for the Asia Pacific region.
Tensile Modulus 3.55 GPa

@Temperature 120 °C
515 ksi

@Temperature 248 °F
ISO Data
BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Dry)
Ultramid 8233G HS is a heat stabilized, 33% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. It is also..
Tensile Modulus 3.55 GPa
515 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Valox® K4530 PBT
15% glass reinforced PBT, Hydrolytically stable, High flow, Automotive connectors.
Tensile Modulus 3.55 GPa
515 ksi
Radici Radiflam® A AE (dry) Nylon 66
Radiflam® A is a range of flame retardant polyamides 66 (PA 66) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici g..