Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.55 - 3.65 GPa | 515 - 529 ksi | ASTM D638 |
Prodways PLASTCure ABS 3650 3D Printing Polymer Good chemical resistance. High transparency.Ideal for segments such like medical, electronic, aerospace and automotive markets that demand accurate RTV patterns, durable concept models, highly accur.. |