Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.58 GPa | 519 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP COLORCOMP EX12304C PEI (Asia Pacific) LNP* Colorcomp* EX12304C is an unfilled polyetherimide clean compound with extremely high level of cleanliness for the most demanding application. This compound is manufactured using LNP CCS technol.. |
|||
Tensile Modulus | 3.58 GPa | 519 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 1000F PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact Compliant, NSF 51 Listing. Effective June, 2007 this grade will no long.. |
|||
Tensile Modulus | 3.58 GPa | 519 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 1000F PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June 2007, this grade will no longer.. |
|||
Tensile Modulus | 3.58 GPa | 519 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem 1000FV PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact Compliant, NSF 51 Listing.This data wa.. |
|||
Tensile Modulus | 3.58 GPa | 519 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem 1000FV PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact Compliant, NSF 51 Listing.This data wa.. |
|||
Tensile Modulus | 3.58 GPa | 519 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem 1000M PEI Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 3.58 GPa | 519 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem 1000M PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 3.58 GPa | 519 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 1000P PEI Standard flow Polyetherimide (Tg 217C) in 350 micron powder. ECO Conforming. |
|||
Tensile Modulus | 3.58 GPa | 519 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 1000P PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C) in 350 micron powder. ECO Conforming. |
|||
Tensile Modulus | 3.58 GPa | 519 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 1000R PEI Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0, V2 and 5VA listing. |
|||
Tensile Modulus | 3.58 GPa | 519 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem 1000RV PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Europe-Afr.. |
|||
Tensile Modulus | 3.58 GPa | 519 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 1010 PEI Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June 2007, this grade will no longer b.. |
|||
Tensile Modulus | 3.58 GPa | 519 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 1010 PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June 2007, this grade will no longer be .. |
|||
Tensile Modulus | 3.58 GPa | 519 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 1010F PEI Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contant compliant, NSF 51 listing. Effective June 2007, this grade will no longer b.. |
|||
Tensile Modulus | 3.58 GPa | 519 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 1010F PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contant compliant, NSF 51 listing. Effective June 2007, this grade will no longer be .. |
|||
Tensile Modulus | 3.58 GPa | 519 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem 1010FV PEI Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contant compliant, NSF 51 listing.This data wa.. |
|||
Tensile Modulus | 3.58 GPa | 519 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem 1010FV PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contant compliant, NSF 51 listing.This data wa.. |
|||
Tensile Modulus | 3.58 GPa | 519 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem 1010FV PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contant compliant, NSF 51 listing.This data wa.. |
|||
Tensile Modulus | 3.58 GPa | 519 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 1010M PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. |
|||
Tensile Modulus | 3.58 GPa | 519 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 1010R PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Tensile Modulus | 3.58 GPa | 519 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 1010R PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Tensile Modulus | 3.58 GPa | 519 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 1010TC PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing. |
|||
Tensile Modulus | 3.58 GPa | 519 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem 1010V PEI Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing.This data wa.. |
|||
Tensile Modulus | 3.58 GPa | 519 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem 1010V PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing.This data wa.. |
|||
Tensile Modulus | 3.58 GPa | 519 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 1010X PEI Enhanced flow Polyetherimide (Tg 217C) with low ionic contamination of less than 0.1 ppm each of leachable chloride and sulphates. ECO Conforming. Factory Mutual FM4910 compliant in recognized col.. |
|||
Tensile Modulus | 3.58 GPa | 519 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM HU1000 PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |
|||
Tensile Modulus | 3.58 GPa | 519 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM HU1010 PEI Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI),.. |
|||
Tensile Modulus | 3.58 GPa | 519 ksi | Storage |
Epoxy Technology EPO-TEK® E4110 Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® E4110 is an electrically conductive, silver-filled epoxy paste. This two component system is designed for low temperature curing from ambient to 80°C, although other.. |
|||
Tensile Modulus | 3.58 GPa | 519 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 1000 PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing, compliant in natural color. Effective June, 20.. |
|||
Tensile Modulus | 3.58 GPa | 519 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 1000 PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June, 2007 this grade will no longer.. |