Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.636 GPa | 527.4 ksi | ISO 527-2/1A/1 |
Lubrizol ESTALOC® 59300 Ester-Type, Reinforced Engineering Thermoplastic (European Grade) Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio.. |