Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 3.73 GPa
541 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP PL002 PA 6
LNP* LUBRICOMP* PL002 is a compound based on Nylon 6 base resin containing 10% PTFE. Added feature of this grade is: Wear Resistant.
Tensile Modulus 3.73 GPa
541 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Lubricomp RL001 PA 66
LNP Lubricomp* RL001 is a Nylon 6/6 base resin containing PTFE lubricant. Characteristics are internally lubricated.This data was supplied by SABIC-IP for the Americas region.
Tensile Modulus 3.73 GPa
541 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON EX11402 PEI
LNP* STAT-KON* EX11402 is a compound based on Polyetherimide resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
Tensile Modulus 3.73 GPa
541 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Thermocomp DX99721 PC
LNP* Thermocomp* DX99721 is a compound based on Polycarbonate resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Tensile Modulus 3.73 GPa
541 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Thermocomp DX99721 PC (Asia Pacific)
LNP* Thermocomp* DX99721 is a compound based on Polycarbonate resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
Tensile Modulus 3.73 GPa
540 ksi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® VG-4910 ABS, Glass Filled FR
Information provided by Samsung Cheil Industries.
Tensile Modulus 3.73 GPa
540 ksi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® VG-4910 ABS, Glass Filled FR
Information provided by Samsung Cheil Industries.
Tensile Modulus 3.73 GPa
541 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP XFL21R PA
LNP* LUBRICOMP* XFL21R is a compound based on Amorphous Nylon resin containing 5% Glass Fiber, 10% PTFE. Added features of this material include: Wear Resistant, Mold Release.
Tensile Modulus 3.73 GPa

@Temperature -100 °C
541 ksi

@Temperature -148 °F
DAM; Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Zytel® ST801 BK010A Nylon 66  (Unverified Data**)
Super Toughened Polyamide 66 Information provided by DuPont Performance Polymers
Tensile Modulus 3.73 GPa

@Temperature -40.0 °C
541 ksi

@Temperature -40.0 °F
ISO Data
BASF Ultramid® 8202CQ PA6 (Dry)
Ultramid 8202CQ is a low viscosity, PA6 injection molding homopolymer, possessing a modified crystalline structure or increased property performance and faster cycles. It is also available in pigme..