Material Notes:
LNP* Thermocomp* DX99721 is a compound based on Polycarbonate resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Physical Properties Metric English Comments
Density 1.28 g/cc
0.0462 lb/in³
ASTM D 792
Linear Mold Shrinkage, Flow 0.0070 cm/cm

@Time 86400 sec
0.0070 in/in

@Time 24.0 hour
ASTM D 955
Mechanical Properties Metric English Comments
Tensile Strength at Break 67.0 MPa
9720 psi
ASTM D 638
Elongation at Break 4.1 %
4.1 %
ASTM D 638
Tensile Modulus 3.73 GPa
541 ksi
50 mm/min; ASTM D 638
Flexural Strength 110 MPa
16000 psi
ASTM D 790
Flexural Modulus 3.48 GPa
505 ksi
ASTM D 790
Izod Impact, Notched 0.740 J/cm

@Temperature 23.0 °C
1.39 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Izod Impact, Unnotched 9.92 J/cm

@Temperature 23.0 °C
18.6 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 139 °C

@Thickness 3.20 mm
282 °F

@Thickness 0.126 in
unannealed; ASTM D 648