Polymer Property : Tensile Modulus = 3100 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 21.4 GPa

@Temperature 23.9 °C
3100 ksi

@Temperature 75.0 °F
Dry; ASTM D3039
Park Electrochemical Nelcote® E-766B Epoxy Prepreg, 7581 E-Glass Reinforced
Nelcote® E-766B is a low tack, self adhesive epoxy resin system designed for honeycomb applications. E-766B displays excellent peel properties.Key Features and Benefits:Self adhesive resin system f..
Tensile Modulus 21.4 GPa
3100 ksi
MTI ThermoStran® PA66-60G Long Glass Fiber Compound
ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t..
Tensile Modulus 21.4 GPa
3100 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP SCL36 PA12
LNP* LUBRICOMP* SCL36 is a compound based on Nylon 12 resin containing 15% PTFE, 30% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive.