Mechanical Properties Metric English Comments
Tensile Modulus 340 GPa
49300 ksi
Young's; DINV ENV 843-2 / ASTM-F417
CeramTec Rubalit® 708S Alumina, 96%
Rubalit® 708S (96%) is an alumina that features high strength and thermal conductivity. It provides outstanding results when used on commercially available thick-film pastes and metallization syste..