Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 340 GPa | 49300 ksi | Young's; DINV ENV 843-2 / ASTM-F417 |
CeramTec Rubalit® 708S Alumina, 96% Rubalit® 708S (96%) is an alumina that features high strength and thermal conductivity. It provides outstanding results when used on commercially available thick-film pastes and metallization syste.. |