Polymer Property : Tensile Modulus = 350 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 350 GPa
50800 ksi
Young's; DINV ENV 843-2 / ASTM-F417
CeramTec Rubalit® 710 Alumina, 99.6%
Rubalit® 710 (99.6%) is an alumina that produces optimum results and is considered the material of choice for thin-film technology. Its characterizing features are high strength and thermal conduct..
Tensile Modulus 350 GPa
50800 ksi
Young's; DINV ENV 843-2 / ASTM-F417
CeramTec Rubalit® A 1999.5 Alumina, 99.7%
Rubalit® A 1999.5 (99.7%) is mechanically stronger, features a higher heat conductivity, and is more corrosion resistant than other aluminas. This high-purity aluminum oxide ceramic with carbon mat..
Tensile Modulus 350 GPa
50800 ksi
Young's; DINV ENV 843-2
CeramTec V 38 Alumina, 96.0% Al2O3-SiO2
Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures.
Tensile Modulus 350 - 390 GPa
50800 - 56600 ksi
Goodfellow Ruby, Al2O3
Ruby exhibits identical properties to those of sapphire. Small amounts of impurities, especially chromium oxide, give ruby a red coloration. Useful optical range from 150 - 5500 nm.Information pro..
Tensile Modulus 350 GPa
50800 ksi
Young's
CeramTec Rubalit® A 1896 brown Alumina
CeramTec AG's seal and regulator discs are made mainly of Rubalit® A 1896, a material developed especially for this application that is noted for the following special properties: outstanding hard..