Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 350 GPa | 50800 ksi | Young's; DINV ENV 843-2 / ASTM-F417 |
CeramTec Rubalit® 710 Alumina, 99.6% Rubalit® 710 (99.6%) is an alumina that produces optimum results and is considered the material of choice for thin-film technology. Its characterizing features are high strength and thermal conduct.. |
|||
Tensile Modulus | 350 GPa | 50800 ksi | Young's; DINV ENV 843-2 / ASTM-F417 |
CeramTec Rubalit® A 1999.5 Alumina, 99.7% Rubalit® A 1999.5 (99.7%) is mechanically stronger, features a higher heat conductivity, and is more corrosion resistant than other aluminas. This high-purity aluminum oxide ceramic with carbon mat.. |
|||
Tensile Modulus | 350 GPa | 50800 ksi | Young's; DINV ENV 843-2 |
CeramTec V 38 Alumina, 96.0% Al2O3-SiO2 Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures. |
|||
Tensile Modulus | 350 - 390 GPa | 50800 - 56600 ksi | |
Goodfellow Ruby, Al2O3 Ruby exhibits identical properties to those of sapphire. Small amounts of impurities, especially chromium oxide, give ruby a red coloration. Useful optical range from 150 - 5500 nm.Information pro.. |
|||
Tensile Modulus | 350 GPa | 50800 ksi | Young's |
CeramTec Rubalit® A 1896 brown Alumina CeramTec AG's seal and regulator discs are made mainly of Rubalit® A 1896, a material developed especially for this application that is noted for the following special properties: outstanding hard.. |