Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.495 GPa | 361.9 ksi | ASTM D638-04 |
Objet FullCure® 830 Vero White Resin for Rapid Prototyping Information provided by American Precision Prototyping, LLC |
|||
Tensile Modulus | 2.495 GPa | 361.9 ksi | ASTM D638 |
RedEye On Demand VeroBlack PolyJet™ FC870 for Rapid Prototyping Vero PolyJet Resin (VeroBlue™ FC840 & VeroBlack™ FC870) is a photopolymer resin designed for precise jetting in super fine layers by PolyJet™ Technology, often used in rapid prototyping. Our Vero.. |
|||
Tensile Modulus | 2.495 GPa | 361.9 ksi | ASTM D638 |
RedEye On Demand VeroWhite PolyJet Resin White for Rapid Prototyping Vero PolyJet Resin (VeroBlue™ FC840 & VeroBlack™ FC870) is a photopolymer resin designed for precise jetting in super fine layers by PolyJet™ Technology, often used in rapid prototyping. Our Vero.. |