Polymer Property : Tensile Modulus = 3630 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 25.0 GPa
3630 ksi
ISO 527-2
PolyOne OnForce™ LFT AM-30LCF/001 Grey Polyphthalamide (PPA)
PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. ..
Tensile Modulus 25.0 GPa
3630 ksi
ISO 527
Nilit FRIANYL B63 CV40 Nylon 6.6 for injection molding, 40% carbon fiber reinforced
Nylon 6.6 for injection molding, good conductive and electrostatic properties.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Tensile Modulus 25.0 GPa
3630 ksi
ASTM D638
LNP Thermocomp® LC-1006 EM Polyetheretherketone, Carbon Fiber Reinforcement  (discontinued **)
Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st..
Tensile Modulus 25.0 GPa
3630 ksi
ISO 527
Victrex® PEEK 650CA30 30% Carbon Fiber Filled, PolyEtherEtherKetone
High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, FDA food contact compliant..
Tensile Modulus 25.0 GPa

@Temperature 23.0 °C
3630 ksi

@Temperature 73.4 °F
ISO 527
Victrex® PEEK 90GL60 Polyetheretherketone, 60% Glass Fibre Reinforced
Product Description:High performance thermoplastic material, 60% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, standard flow, FDA food contac..
Tensile Modulus 25.0 GPa
3630 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP OCL36A PPS - Branched (Europe-Africa-Middle East)
LNP* Lubricomp* OCL4036 is a compound based on PPS - Branched resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive.
Tensile Modulus 25.0 GPa

@Temperature 100 °C
3630 ksi

@Temperature 212 °F
90º, Wet; EN2561
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, 37%/7781 Fiber
Information provided by HexCel
Tensile Modulus 25.0 GPa
3630 ksi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® GVX-65 H black 9915 PA*-GF65
Product description: Grivory GVX-65H black 9915 is a 65% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolya..
Tensile Modulus 25.0 GPa
3630 ksi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® GVX-65 H nat PA*-GF65
Product description: Grivory GVX-65H natural is a 65% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyami..
Tensile Modulus 25.0 GPa
3630 ksi
ISO 527
Eurotec® Tecomid® NT40 CR30 BK111 HS PPA, 30% carbon fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
Tensile Modulus 25.0 GPa
3630 ksi
longitudinal; ISO 527-4/5
Bond Laminates TEPEX® dynalite 108-FGAL290(1)-FG290(x)/45% Filament Glass – TPU Consolidated Composite Laminate
Within the TEPEX® composite laminate, TPU distinguishes itself from alternative resin systems by its specific physical properties. The TPU resin is tough which results in an excellent impact and ea..
Tensile Modulus 25.0 GPa
3630 ksi
longitudinal; ISO 527-4/5
Bond Laminates TEPEX® dynalite 108-FGAL290(2)-FG290(x)/45% Filament Glass – TPU Consolidated Composite Laminate
Within the TEPEX® composite laminate, TPU distinguishes itself from alternative resin systems by its specific physical properties. The TPU resin is tough which results in an excellent impact and ea..
Tensile Modulus 25.0 GPa
3630 ksi
longitudinal; ISO 527-4/5
Bond Laminates TEPEX® dynalite 108-FG290(x)/45% Filament Glass – TPU Consolidated Composite Laminate
Within the TEPEX® composite laminate, TPU distinguishes itself from alternative resin systems by its specific physical properties. The TPU resin is tough which results in an excellent impact and ea..
Tensile Modulus 25.0 GPa
3630 ksi
EN2597B
Hexcel® HexPly® M56 180°C (350°F) Out-of-Autoclave Curing Matrix, M56/37%/7581
Fiber: E-Glass, Weave: 8HS, 300 g/m2Information provided by HexCel