Mechanical Properties Metric English Comments
Tensile Modulus 25.4 GPa
3680 ksi
ISO 527-2/1A/1
Solvay Specialty Polymers KetaSpire® KT-880 CF30 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-880 CF30 is a high flow, 30% carbon fiber reinforced grade of polyetheretherketone (PEEK). Carbon-fiber reinforcement of KetaSpire PEEK provides the maximum levels of mechanical propert..
Tensile Modulus 25.4 GPa
3680 ksi
1 mm/min, Type 1A; ISO 527-2
Solvay Specialty Polymers KetaSpire® KT-880 CF30 Polyetheretherketone (PEEK), 30% Carbon Fiber
KetaSpire® KT-880 CF30 is a high flow, 30% carbon fiber reinforced grade of polyetheretherketone (PEEK). Carbon-fiber reinforcement of KetaSpire® PEEK provides the maximum levels of mechanical..