Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.75 GPa | 399 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CX7010 PC+ABS (Asia Pacific) Cycoloy* CX7010 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0. Excellent flow combined with good balance of pro.. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CY5100 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering excellent flow / impact balance for large size applications |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CY5100 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering excellent flow / impact balance for large size applicationsThis data was supplied by SABIC-IP .. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CY6110 PC+ABS (Asia Pacific) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Geloy FXTW30PE ASA Pearlescent GELOY ASA resin with copper-look for capstock extrusion. Outstanding weatherability.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® SLX2432D PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East reg.. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DAL22 PC LNP* Lubricomp* DAL22 is a compound based on Polycarbonate resin containing 10% PTFE and 10% Aramid Fiber. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | STN EN ISO 527-2 |
Plastcom SLOVAMID 6 LI/1 Polyamide 6, Impacted FeaturesPA 6 with the content of thermoplastic elastomer. Impacted, for mouldings with high toughness either at low temperatures, suitable for external use, eg. ski shoes, sports and safety helmets.. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Geloy FXTW30CP ASA Pearlescent GELOY ASA resin with copper-look for capstock extrusion. Outstanding weatherability.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® XHT4143 PC Copolymer (Europe-Africa-Middle East) XHT4143 is a high flow, UV stabilized, high heat polycarbonate copolymer blend with an HDT/Af of 162C. It is available in a range of opaque and limited transparent colors. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | |
Green Dot Terratek® WC 100300 Polypropylene - Pine Fiber Composite Terratek® WC 100300 is a proprietary blend of pine wood fiber and reprocessed polypropylene for injection molding applications. WC 100300 contains 30% wood fiber by weight, however, a range of pr.. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP EL003 PEI LNP LUBRICOMP* EL003 is a compound based on Polyetherimide resin containing 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP EL003 PEI (Europe-Africa-Middle East) LNP LUBRICOMP* EL003 is a compound based on Polyetherimide resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP KL001 Acetal Copolymer LNP* LUBRICOMP* KL001 is a compound based on Acetal Copolymer resin containing 5% PTFE. Added feature of this material is: Wear Resistant. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP KL004L Acetal Copolymer LNP* LUBRICOMP* KL004L is a compound based on Acetal Copolymer resin containing 20% PTFE. Added features of this material include: Wear Resistant, Low Extractible. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP RP003 PA 66 (Asia Pacific) LNP* Lubricomp* RP003 is a compound based on Nylon 66 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP RP004 PA 66 (Asia Pacific) LNP* Lubricomp* RP004 is a compound based on Nylon 66 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP ZI001XXX PPE+PS (Asia Pacific) LNP* Lubricomp* ZI001XXX is a compound based on PPE+PS Blend resin. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DX05499 PC (Asia Pacific) LNP STAT-KON* DX05499 is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP AF001H ABS LNP* THERMOCOMP* AF001H is a compound based on ABS resin containing 5% Glass Fiber. Added feature of this material is: Healthcare. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP AF001H ABS (Asia Pacific) LNP* Thermocomp* AF001H is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | ISO 527 |
Eurotec® Tecomid® NT40 NL MB PPA, impact modified, heat stabilized, natural Information provided by Eurotec® |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | ISO 527-1 |
Barlog Plastics KEBAFORM C 130 HD POM Copolymer unreinforced, improved fuel resistance POMInformation provided by BARLOG plastics GmbH. |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | ISO 527-1/-2 |
BASF Ultraform® W2320 U03 POM Description: Very free-flowing, rapidly solidifying grade with UV stabilization for use where processing is extremely difficult but mechanical requirements are lower.Information provided by BASF |
|||
Tensile Modulus | 2.75 GPa | 399 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON MFD02 PP (Asia Pacific) LNP* Stat-kon* MFD02 is a compound based on Polypropylene resin containing Glass Fiber, Carbon Powder. Added features of this material include: Electrically Conductive. |