Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.0300 GPa | 4.35 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® SC948 NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester Elastomer Developed for the Healthcare Industry Hytrel SC948 NC010 is a low modulus grade with nom. durometer hardness of 40D contains non-discoloring stabilize.. |
|||
Tensile Modulus | 0.0300 GPa | 4.35 ksi | average; in the plane; ISO 527 1-2 |
3A Composites Core Materials AIREX® R63.50 Damage Tolerant Foam AIREX® R63 is a closed-cell, linear, thermoplastic polymer foam with high damage tolerance. This one of a kind formula combines very high elongation and excellent bond strength. AIREX® R63 is cold.. |
|||
Tensile Modulus | >= 0.0300 GPa | >= 4.35 ksi | ASTM D4745-97 |
Adamas Adalon® 413 PTFE, 20% PPS Information provided by Adamas, HPM |
|||
Tensile Modulus | 0.0300 GPa | 4.35 ksi | |
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Tensile Modulus | >= 0.0300 GPa | >= 4.35 ksi | in the plane; ISO 527 1-2 |
3A Composites Core Materials AIREX® C71.55 Elevated Temperature Structural Foam AIREX® C71 is a closed cell, crosslinked polymer foam especially formulated to maintain its stability also at higher processing or service temperatures. It combines excellent stiffness and strength.. |